著者
佐々木 直彦 桃野 正
出版者
一般社団法人 日本鉄鋼協会
雑誌
鉄と鋼 (ISSN:00211575)
巻号頁・発行日
vol.93, no.12, pp.792-798, 2007-12-01 (Released:2009-02-13)
参考文献数
6
被引用文献数
3 3

The Japanese sword has excellent strength-toughness balance given by two traditional processes. One process is compounding of inner tough iron and outer strong steel. And the other process is cooling-rate control quenching by using thickness of clay-coating before quenching. However, it is a precondition for acquiring high strength-toughness that carbon content of sword parts are regulated in proper quantities. Carbon content of sword parts is very important and controlled under forging process which contains TSUMI-WAKASHI (forge-welding piled steel chips) work and fold-forging.Therefore, changes in carbon content of TAMA-HAGANE steels and carbon steels under traditional forging process were investigated in this study. Changes in carbon content depended on enclosing decarburized or carburized surface in steel as forge-weld interface. Total changes in carbon content were proportional to total layers of included surface in steel. Changes in carbon content per one forge-welded layer. “d (mass%/layer)” was ruled by carbon content of raw materials “C0 (mass%)”. When C0 is over 0.2 mass%, carbon content of forged steel is decreasing and the more C0, the more |d |. C0 is under 0.2 mass%, carbon content is increasing. The mass of forged steels is 4% increasing per one fold-forging cycle, but d is not affected by changes in mass of them.

言及状況

外部データベース (DOI)

Yahoo!知恵袋 (1 users, 1 posts)

俵国一氏の「日本刀の科学的研究」・・・ 冶金の世界ではどのように評価されているのですか? 「日本刀の科学的研究」・・・ これは論文と思っていたのですが、そうではないようです。 説明に不備がありますし、 思い込みによる想像があるようです。 俵 国一氏は、 「俵 国一 小伝」 https://www.isij.or.jp/commendation/?action=common_d ...

Twitter (3 users, 3 posts, 0 favorites)

折り返し鍛錬によって炭素含有量が減少し、15回まで直線的に減少すると https://t.co/8G0le8KYqO

収集済み URL リスト