Nine different food cans, packed with water, were heat-treated for 30 min at 80 or 100°C in order to elucidate the trends associated with the leaching of bisphenol A (BPA) from internal coatings. Low levels of BPA were detected in water from all unheated cans, rising to 0.06 to 32 ng/cm2 after heating at 100°C. Reducing the heat-treatment temperature to 80°C was found to reduce the BPA concentration in the contained water by up to two-thirds. The cans that recorded the highest BPA concentrations in water after heating were found to have components (lid, bottom or body) with high available BPA contents.