- vol.54, no.4, pp.791-800, 2014-04-15 (Released:2014-06-05)
- 参考文献数
- 31
- 被引用文献数
-
11
16
In the recent operation of blast furnace, it is supposed that high gas permeability of burden is important for low RAR and high PCR operation. In this work, sinter quality for improvement in gas permeability of blast furnace was investigated with reduction degradation and under-load-reduction tests. As the results, the reduction degradation of sinter is deteriorated by increasing H2 concentration in the reduction gas under the condition of below 3.8 vol% H2. However, over 3.8 vol% H2, increase of H2 has no effect on the reduction degradation because the diffusion of reduction gas in the sinter is limited. On the other hand, from the under-load-reduction test, there is possibility that increase in H2 concentration of reduction gas and decrease in slag ratio in sinter are effective to improve gas permeability of lower part of blast furnace rather than reducibility of sinter. Due to adoption of these experimental results to a 2-dimentional mathematical simulation model, the precision of pressure drop calculation of blast furnace was improved. It is considered from the evaluation by this model calculation that the RDI, a slag ratio and the slag viscosity as the sinter properties are greatly influence on the permeability of blast furnace.